Effect of Addition of GNMPs on Durability Properties of Locally Produced Sustainable Ultra High Performance Concrete
Description
This FYP, conducted by Muhammad Akif, Muhammad Huzaifa Saddique, and Talal Hassan at COMSATS University Islamabad (Wah Campus) under Engr. Raja Tassadiq, investigates the durability of Reactive Powder Concrete (RPC) using locally available Pakistani materials, incorporating crumb rubber from waste tyres as a partial sand replacement and Graphite Nano/Micro Platelets (GNMPs) as filler. Twelve mixes were tested for water absorption, acid resistance, marine exposure, and sorptivity per ASTM standards. Mix M6 (5% rubber + 0.3% GNMPs) delivered the best durability, while 15% rubber negatively impacted performance. The study supports sustainable construction by addressing sand depletion and waste tyre disposal, aligning with UN SDGs 9, 11, 12, and 13.
Objectives
1. Develop a Sustainable RPC Mix Design — To formulate a Reactive Powder Concrete mix using locally available Pakistani materials, with crumb rubber used as a partial sand replacement at levels of 0%, 5%, 10%, and 15%. 2. Investigate the Effect of GNMPs — To study the impact of Graphite Nano/Micro Platelets (GNMPs), added at 0.1%, 0.2%, and 0.3% by weight of cement, on the durability properties of rubberized RPC. 3. Evaluate Durability Performance — To assess the developed mixes through four key durability tests: water absorption, marine water exposure, acid environment exposure, and sorptivity. 4. Identify the Optimum Mix — To determine the best combination of crumb rubber replacement level and GNMPs dosage that delivers the highest overall durability performance.
Socio-economic benefit
1. Solving Pakistan's Sand Scarcity Crisis Pakistan consumes an estimated 50 million tonnes of concrete annually, placing enormous pressure on natural river sand resources. This project offers a practical alternative by replacing natural sand with crumb rubber, helping reduce unsustainable sand mining from major rivers like the Indus, Jhelum, and Chenab — which is causing riverbank erosion, habitat loss, and falling groundwater levels. 2. Waste Tyre Disposal & Public Health Around 2–3 million waste tyres are burnt or dumped in riverbeds and landfills across Pakistan each year, releasing toxic gases and creating breeding grounds for mosquitoes that spread diseases like dengue fever. By recycling tyre rubber into construction material, this project directly addresses a major public health and environmental hazard. 3. Low-Cost, Locally Sourced Materials All materials used — crumb rubber, river sand, cement, silica fume, and acacia gum — are locally available in Pakistan. This reduces import dependency, lowers production costs, and makes high-performance concrete more accessible for developing countries. 4. Durable Infrastructure for Developing Nations The optimized RPC mix offers superior resistance to marine water, acid, and water absorption, making it suitable for use in challenging environments such as coastal areas, industrial zones, and sewage infrastructure — directly supporting Pakistan's growing infrastructure needs. 5. Alignment with UN Sustainable Development Goals (SDGs) The project contributes to four UN SDGs: SDG 9 — Resilient infrastructure through innovative materials SDG 11 — Sustainable cities using durable, locally produced UHPC SDG 12 — Responsible consumption by reusing industrial waste (rubber & silica fume) SDG 13 — Climate action by reducing landfill burden and carbon footprint from raw material extraction 6. Circular Economy & Environmental Benefits By diverting waste tyres from landfills into construction, the project promotes circular economy principles, reduces carbon emissions associated with raw material extraction, and contributes to a cleaner, more sustainable construction industry in Pakistan.
Methodologies
Step 1 — Materials Selection Nine locally available materials were used: Ordinary Portland Cement, Silica Fume, Fine River Sand, Crumb Rubber (shredded waste tyres), GNMPs, Acacia Gum (as dispersant), Steel Fibres, Superplasticizer (Chemrite 303 SP), and potable water. Step 2 — Mix Design The mix was designed using the Absolute Volume Method with a water-to-binder ratio of 0.22. A total of 12 mix combinations were prepared by varying crumb rubber (0%, 5%, 10%, 15%) and GNMPs dosage (0.1%, 0.2%, 0.3%). Step 3 — GNMPs Solution Preparation GNMPs were pre-dispersed in water using Acacia Gum on a magnetic stirrer for 24 hours to prevent nanoparticle agglomeration before mixing. Step 4 — Mixing Procedure A Planetary Mixer was used in 5 sequential stages: dry mixing ? crumb rubber incorporation ? GNMPs solution addition ? remaining water addition ? steel fibre addition. Step 5 — Specimen Casting & Curing All specimens were cast as 50×50×50 mm cubes (except sorptivity specimens which were 100mm diameter cylinders) and cured under standard conditions. Step 6 — Durability Testing (ASTM Standards) Four tests were performed on all 12 mixes: Water Absorption — ASTM C642 Marine Water Exposure — ASTM D1141 (Arabian Sea water) Acid Resistance — ASTM C267 (Sulphuric acid immersion) Sorptivity — ASTM C1585 Step 7 — Results & Statistical Analysis Results were analyzed using comparative charts, a normalized multi-criteria performance heatmap, and Spearman Rank Correlation to identify inter-test relationships and determine the optimal mix.
Outcome
1. Water Absorption Mix M9 (10% rubber + 0.3% GNMPs) achieved the lowest water absorption of 0.636%, better than the baseline Mix M1 (1.143%). Rubber content up to 10% combined with higher GNMPs dosage effectively reduces capillary porosity. However, 15% rubber significantly increased water absorption, marking it as outside the acceptable range. 2. Acid Resistance All mixes showed good resistance to sulphuric acid attack. Mix M5 (5% rubber + 0.2% GNMPs) achieved the highest post-acid compressive strength of 58.00 MPa, even surpassing the baseline mix. Mix M6 recorded 43.00 MPa. The optimal GNMPs dosage for acid resistance is 0.2% at 5% rubber content. 3. Marine Water Exposure 11 out of 12 mixes showed less than 0.5% mass loss under marine water exposure, confirming excellent chloride and sulphate resistance. Mix M6 (5% rubber + 0.3% GNMPs) recorded the lowest mass loss among rubberized mixes at -0.236%, making it viable for coastal and marine infrastructure applications. 4. Sorptivity Mix M6 achieved a sorptivity of 0.01743 mm/vs, which is 21% lower than the baseline Mix M1 (0.02218 mm/vs), confirming that 0.3% GNMPs effectively densifies the pore network and reduces capillary water absorption at 5% rubber replacement. 5. Optimum Mix Identified Mix M6 (5% crumb rubber + 0.3% GNMPs) was identified as the overall optimum sustainable mix, delivering the best balanced performance across all four durability tests with the maximum usable waste rubber content. 6. Sustainable Construction Validated The study successfully demonstrated that waste tyre crumb rubber and nano-engineered GNMPs can be used together in UHPC production without significantly compromising durability, supporting sustainable construction aligned with UN SDGs 9, 11, 12, and 13.
Gallery
More from Civil Engineering
Effect of Addition of Graphite Nano Micro Platelets (GNMPs) on Mechanical Properties of Lo…
This FYP at COMSATS University Islamabad (Wah Campus) investigates the mechanical performance of Reactive Powd…
Supervisor: Engr. Raja Tasaddiq
BIM to Augmented Reality: A Standardized Multimodal Deployment Framework for Construction…
The construction industry's digital transformation highlights Building Information Modelling (BIM) as a core m…
Supervisor: Dr. Hassan Ashraf
SPREADSHEETS TO SMART DASHBOARD A COMPARATIVE STUDY OF MANUAL AND BIM-BASED QTO USING VI…
This study develops a fully automated BIM-based workflow for quantity take-off (QTO) and cost estimation. An I…
Supervisor: Dr. Hassan Ashraf
DURABILITY PERFORMANCE OF SELF-COMPACTING CONCRETE INCORPORATING NANO-MICRO GRAPHITE AND P…
This study investigates the durability performance of Self-Compacting Concrete (SCC) incorporating Nano-Micro…
Supervisor: Dr. Adnan Nawaz